Use LEFT and RIGHT arrow keys to navigate between flashcards;
Use UP and DOWN arrow keys to flip the card;
H to show hint;
A reads text to speech;
9 Cards in this Set
- Front
- Back
What can happen if cooling of the pipe below the installation temperature results in excess of tensile force being placed on the piping connection |
Pullout especially from compression joints |
|
What happens to the epoxy after a short period of soaking time |
It forms a cross-link structure and cures as a thermoset plastic liner |
|
What color is associated with PTFE |
White |
|
What will most likely happen if line piping spools are stored in conditions where the ambient temperature may fall below minus 18 degrees Celsius 0 degrees Fahrenheit |
The gasket surface will break off at the end of the liner |
|
What should be done to reduce the moisture content at the weld zone of welded concrete and mortar lined steel piping joint |
Preheat the pipe ends to a temperature of 55 degrees Celsius 130 degrees Fahrenheit |
|
What is the maximum compression allowed on the gasket faces between two rubber lined flanges |
A gasket face should not be compressed more than one-third of the initial thickness |
|
Besides gaskets what must be installed between the faces when joining the flange of line pipe to that of an unlined pipe |
A flat faced spacer ring |
|
What is the most common cause of rejection for a lined piping spool or component in a piping installation |
Liner has been damaged in transit to its position in the assembly |
|
Compare to polypropylene pipe PP lined metal pipe has in broader operating temperature range true or false |
True |