Ductile fractured by... Brittle fractured by... Due to?? In Area |
Necking Crack and crack Propagation |
|
Dynamics mech Prop.. Failure when |
Impact strength Fatigue Dynamic Creep Below YS |
|
Factors Ass with Polymerization |
-Evolution of heat (Exothermic) - Reduction in Volume (Polymerization Shrinkage) - Residual Monomer |
|
Inhibitors added to |
Prevent polymerization during storage and give shelf life |
|
Factors aff polymerization |
|
|
For Good Wetting Should be |
- SE > ST - LOW VISCOSITY |
|
EXAM Grain Boundaries and Grain Proper |
|
|
EXAM Plastic Deformation in metals occ by |
Dislocation Movement |
|
Measure by which dislocation can move in Metal |
PL or YS |
|
EXAM E depend on |
Composition and nature of bonding |
|
Process of heating amorphous to Form crystalline.. Other name |
Devitrification... Ceramming |
|
EXAM Transformation toughening.. Of.. Stimulator... From... To... With Inc in w Inhibition of |
Zirconia Stress Tetragonal Monoclinic Volume... Cracks |
|
Effect of antimicrobial on Prop |
No Effect |
|
EXAM Compaction.. Other name.. Why |
Condensation -To Remove Excess Water - To Shape Plastic Mass - To adapt it to Substructure |
|
Process Responsible for fusion of Powder to form Continuous mass |
Sintering |
|
EXAM Methods of Altering mech Prop |
|