During inspection of an injection point circut, extensive inspection should be conducted downstream of the injection point for a distance at leadt

D 10 pipe diameters

Insulated austenitic stainless steel pipe is susceptible to CUI(Cholride stress corrosion cracking) at temperature range of

D 120-400°F

Track wels should be

A made by a qualified welder or welding operator