What is determined by the sharpness of the penetrometer holes?
|
Detail sensitivity
|
|
According to military standards, what is the radiographchic quality level if no specifications are available ? |
2-2T |
|
The penetrometer holes have sharp boundaries and give an abrupt change in metal ?
|
Thickness |
|
When using lead screens where is the film placed?
|
Between a pair of screens |
|
What determines the intensity of fluorescent light emitted by a fluorescent screen? |
Intensity of incident radiation
|
|
What is the function of the diaphragm in radiography ?
|
Confines the primary beam
|
|
By applying geometric factors to your radiographic images, you are able to control distortion, sharpness, and degree of |
enlargement |
|
Which geometric factor is not controllable by the operator?
|
Energy source size
|
|
What is the name of the graph showing the relationship between material thickness, kilo voltage, and exposure?
|
Technique Chart
|
|
What aid is necessary to use a densitometer for making exposure corrections?
|
To establish a starting density from which to correct |
|
The film characteristics curves are used to |
computer exposure corrections |
|
Film characteristic curves show that M film is
|
slower than AA |
|
The area distance formula expresses what relationship?
|
Area covered by the primary beam increases as source to object distance increases |
|
What type of defect is normally distinguished by a dark continuous jagged or straight line throughout its length on a radiograph? |
Crack |
|
Which technique can pinpoint the location of a crack? |
Triangulation |
|
Which radiographic defect appears as smooth, consistent, light density, areas that do not have a grainy or porus appearance ?
|
Water in honey comb core |
|
During welder certification, what type of defect automatically results in an unacceptable weld if it exceeds certain limits ?
|
Linear defects |
|
What items are required under the penetrometer when x-raying welding certification plates? |
Shim |
|
Which discontinuity appears as a dark irregular line offset from the centerline of the weldment ?
|